Cita de ítemdc.identifier.citationJOURNAL OF MATERIALS PROCESSING TECHNOLOGY Volume: 173 Issue: 3 Pages: 352-358 Published: APR 20 2006en
Identifierdc.identifier.issn0924-0136
Identifierdc.identifier.urihttps://repositorio.uchile.cl/handle/2250/124763
Abstractdc.description.abstractIn this study, the abrasive wear resistance of previously boronized 1020, 1045, 4140 and 4340 steels were determined. The boronizing treatments were performed in a mixture of dried borax and SiC at temperatures of 1223, 1273 and 1323 K, during 2, 4 and 8 h. On the surface of each steel, a monophase layer of Fe2B was obtained. The abrasive wear tests were performed by using a rubber-wheel apparatus (ASTM-G65 standard) operating with quartz sand and a force between wheel and specimen of 130N. As a result, boronized 1020 steel exhibited the greatest abrasive wear resistance.en
Lenguagedc.language.isoenen
Publisherdc.publisherELSEVIERen
Keywordsdc.subjectBEHAVIORen
Títulodc.titleAbrasive wear resistance of boronized carbon and low-alloy steelsen