(2003)The new quaternary selenophosphate phases AMP2Se6 (A ¼ Cu, Ag and M ¼ Bi, Sb) were synthesized by ceramic methods at 1023 K. These phases were characterized by powder X-ray diffraction (XRD), Fourier transform infrared ...
-
(2003)The new quaternary selenophosphate phases AMP2Se6 (A = Cu, Ag and M = Bi, Sb) were synthesized by ceramic methods at 1023 K. These phases were characterized by powder X-ray diffraction (XRD), Fourier transform infrared ...